1 L and 10 L batchtype wet grinding stirred media mills. The employed grinding media was zirconia (ZrO 2) beads with a density of 6 g/cc and mean diameter of mm. Grinding experiments were conducted under different rotational speeds of the rotor. The investigated rotational speeds varied from 360 to 800 rpm for each type of mill.